Energetic Materials and Tungsten Alloys Interface Machining with Femtosecond Laser
ID:84 View Protection:ATTENDEE Updated Time:2024-04-22 23:49:37 Hits:306 Poster Presentation

Start Time:Pending(Asia/Shanghai)

Duration:Pending

Session:No Session »

No files

Abstract
Abstract
Objective:
The interfacial interaction properties of femtosecond lasers with energetic materials (EMs) and metal shells were studied during disassembling of decommissioned EMs. Based on verifying the safety of femtosecond processing of a single type of explosives, analyzing the safety processing parameters of explosives bonded to tungsten alloys. This research will develop the theory of femtosecond laser-materials interactions, providing an efficient way to disassemble decommissioned munitions.
Methods:
The femtosecond laser used for explosive ablation and cutting in the experiment is a Ti: sapphire laser with a center wavelength of 800 nm, a pulse width of 35 fs, a pulse repetition frequency of 1000 Hz, and average output power of 2 W. The explosion-proof tank is carried out during the EMs cutting process, which can contain the pressure pulse, high temperature, and reaction debris generated by the explosion and filter the harmful gas during the laser cutting. The bottom three-dimensional motion control platform moves the EMs samples, and the charge coupled device (CCD) camera observes and records the reaction phenomenon of the sample ablation and cutting through the window of the explosion-proof tank. This work ensures the safety of the experimental process by strictly controlling the number of explosives (mg level).
Results and Discussions
The results of the ablation experiment were detected by microscopic detection methods, and the ablation characteristics of tungsten alloys and explosive were discussed. When the incident fluence of the femtosecond laser is 0.32 J/cm2, regular elliptical holes are formed on the surface of the TATB and the surface layer appears black. This morphology indicates that the femtosecond laser irradiation will not cause obvious thermal effects on the area outside the laser irradiation area at low fluence. The ablation area and contour are black when the incident laser fluence is in the lower range of 0.32 – 1.59 J/cm2. With the high incident laser fluence, the ablation area expands rapidly, but the surrounding area yellowed by the influence of heat is not obvious. When the laser energy range is within 3.19 – 6.37 J/cm2, we can find the ablation area is significantly larger than the laser spot area. Compared with the increase of laser fluence from 0.32 J/cm2 to 6.37 J/cm2, the ablation area of TATB has risen by about 30 times, and the surrounding heat-affected material is denatured, while the ablation area of HMX has increased by three times and the ablation morphology has no obvious change.
Conclusions
In summary, we demonstrated the feasibility and safety of femtosecond laser cutting of metal alloy of discarded ammunition by femtosecond laser single-pulse irradiation. Under laser single-pulse irradiation, HMX is more stable than TATB without significant thermal effect, even when the laser fluence reaches 6.37 J/cm2. Femtosecond laser fluence between 0 – 3.19 J/cm2 is a safe working range for cutting tungsten-bonded TATB and HMX. The research of femtosecond laser cutting provides a theoretical basis for the disassembly and precision machining of energetic materials, which can effectively reduce the occurrence of dangerous accidents in the process of discarded ammunition.
 
Keywords
femtosecond laser,tungsten alloy,energetic materials,safety verification
Speaker
静轩 王
中国工程物理研究院激光聚变研究中心

Submission Author
静轩 王 中国工程物理研究院激光聚变研究中心
Submit Comment
Verify Code Change Another
All Comments
Important Date
  • Conference Date

    May 13

    2024

    to

    May 17

    2024

  • Mar 31 2024

    Registration deadline

  • Apr 15 2024

    Abstract Submission Deadline

Sponsored By
National Key Laboratory of Shock wave and Detonation Physics
School of Physics, Zhejiang University
Pulsed Power Technology and Application Association of Chinese Nuclear Society
Contact Information